Views: 4 Author: Site Editor Publish Time: 2021-09-17 Origin: Site
Usage and precautions of date batch code stamp:
Please adjust the printer pressure and printing temperature according to the printing speed at the same time to make the printing effect to the best state. If there is no temperature display, it can be adjusted according to the ambient temperature and service conditions, and the possible problems of the product during use are analyzed:
1. The edge of the printing font is fuzzy or empty core. The main reason is that the temperature is too high or the pressure of the printer is too heavy. Please adjust the temperature and pressure of the printer at the same time to optimize the printing effect.
2. The main reasons for the incomplete printing font: low printing temperature, too light pressure of the coder or irregular arrangement of words. Please try to adjust the temperature, pressure of the coder or rearrange the words to achieve the best printing effect.
3. Each time you turn on the printer or change the word grain, please preheat the printer for 20-30 minutes (if the temperature of the printer does not rise, please submit it to professional personnel for maintenance)
4. After each date adjustment, the characters shall be arranged neatly with the same height.
5. High temperature or irregular arrangement of characters are the main reasons for the broken band.
To meet the requirements of different printed materials and durability, heat transfer ribbons can be divided into wax based and resin based according to the coating materials.
a. Wax base: it usually has high density, high sensitivity, leather application, excellent printing effect and low cost.
b. Resin base: the most durable, wear-resistant, heat-resistant, some formulas can prevent steam pressure, etc. According to the model of the code printer, date batch code stamp has different width, length and other specifications.